Grease | AP101 ![]() | AP100 ![]() | M ![]() | N ![]() |
Main Application | General use | Lubricating | High vacuum | General vacuum |
Melting Point ASTM.D 566 | >200°C | 42-52°C | 40-60°C | 42-52°C |
Working temp. range | -40 to180°C | 10 to 30°C | 10 to 30°C | -269 to 30°C |
Vapor Pressure (@20°C) | <1.0x10-5 Torr | 7.0x10-11 Torr | 1.7x10-9 Torr | 6x10-10 Torr |
Relative Density (@20°C) | 0.981 | 1.042 | 0.894 | 0.911 |
Radiation Resistance | No | No | Yes | No |
Outgassing Characteristics TML ASTMS .E 595-90 | - | <1.0% | - | <1.0% |
Lubricity 4 Ball Test ASTM .D 2763 (IP 239) | 450kg | 450kg | 140kg | 150kg |
Viscosity of molten grease (@ 50°C / @ 100°C) | - | - | 413cp | - |
- | - | 29.8cp | - | |
Coefficient of expansion per °C over 20°C-30°C | 0.00066 | - | 0.00075 | 0.00072 |
Thermal conductivity | - | - | 0.194w/m°C | 0.194w/m°C |
- | - | - | 0.095w/m°C | |
Latent heat of fusion | - | - | 18.7cal/g | 15cal/g |
Fusion Peak | - | - | 34°C | 31°C |
Vol. resistivity | - | - | 2.6x1016cm | 2.0x1016cm |
Permittivity | - | - | 2.1 | 2.3 |
Loss tangent | - | - | <0.0001 | <0.0001 |
Surface breakdown at flash over | - | - | 28kV | 27kV |
Electric strength | - | - | 850V | 820V |
Grease | H ![]() | L ![]() | T ![]() | PFPE 501 ![]() |
Main Application | Cryogenic | High temps | Medium temps | High temps/lubricating |
Melting Point ASTM.D 566 | does not melt | 42-52°C | 112-137°C | |
Working temp. range | -10 to 240°C | 10 to30°C | 10 to 120°C | -15 to 250°C |
Vapor Pressure (@20°C) | 1.7x10-9 Torr | 7x10-11 Torr | 4.6x10-9 Torr | 1.3x10-12 Torr |
Relative Density (@20°C) | 0.918 | 0.896 | 0.912 | 2.003 |
Radiation Resistance | No | Yes | No | |
Outgassing Characteristics TML ASTMS .E 595-90 | <1.0% | <1.0% | - | <1.0% |
Lubricity 4 Ball Test ASTM .D 2763 (IP 239) | 250kg | 150kg | - | 800kg |
Viscosity of molten grease (@ 50°C / @ 100°C) | - | 766cp | - | |
- | 62.3cp | - | ||
Coefficient of expansion per °C over 20°C-30°C | - | 0.00076 | 0.00073 | |
Thermal conductivity | - | 0.216w/m°C | - | |
- | - | - | ||
Latent heat of fusion | - | 15.1cal/g | - | |
Fusion Peak | 25°C | 32°C | * | |
Vol. resistivity | - | 1.2x1016cm | 3.3x1012cm | |
Permittivity | - | 2.3 | 2.3 | |
Loss tangent | - | <0.0001 | <0.0001 | |
Surface breakdown at flash over | - | 24kV | 24kV | |
Electric strength | - | 730V | 730V |